Everything about Eutectic Point totally explained
The
melting point of a mixture of two or more solids (such as an
alloy) depends on the relative proportions of its ingredients. A
eutectic or
eutectic mixture is a mixture at such proportions that the melting point is as low as possible, and that furthermore all the constituents crystallize simultaneously at this temperature from molten liquid solution. Such a simultaneous crystallization of a eutectic mixture is known as a
eutectic reaction, the temperature at which it takes place is the
eutectic temperature, and the composition and temperature at which it takes place is called the
eutectic point.
The term comes from the
Greek eutektos, meaning 'easily melted.'
The equilibrium
phase diagram at the right displays a simple binary system composed of two components, A and B, which has a eutectic point. The phase diagram plots relative concentrations of A and B along the horizontal axis, and
temperature along the vertical axis. The eutectic point is the point at which the
liquid phase L borders directly on the
solid phase α + β (a homogeneous composed of both A and B), representing the minimum melting temperature of any possible alloy of A and B.
Not all binary system alloys have a eutectic point: those that form a
solid solution at all concentrations, such as the
gold-
silver system, have no eutectic. An alloy system that has a eutectic is often referred to as a eutectic system, or eutectic alloy.
Solid products of a eutectic reaction can often be identified by their
lamellar structure, as opposed to the
dendritic structures commonly seen in non-eutectic solidification. The same conditions that force the material to form lamellae can instead form an
amorphous solid if pushed to an extreme.
Metallic eutectics
The term is often used in
metallurgy to describe the
alloy of two or more component materials having the relative concentrations specified at the eutectic point. When a non-eutectic alloy freezes, one component of the alloy
crystallizes at one temperature and the other at a different temperature. With a eutectic alloy, the mixture freezes as one at a single temperature. A eutectic alloy therefore has a sharp melting point, and a non-eutectic alloy exhibits a plastic melting range. The phase transformations that occur while freezing a given alloy can be understood using the phase diagram by drawing a vertical line from the liquid phase to the solid phase on a phase diagram; each point along the line describes the composition at a given temperature.
Some uses include:
Other eutectic mixtures
Sodium chloride and
water form a eutectic mixture. It has a eutectic point of −21.2 C and 23.3% salt by weight. The eutectic nature of salt and water is exploited when salt is spread on roads to aid
snow removal, or mixed with ice to produce low temperatures (for example, in traditional
ice cream making).
Lidocaine and
prilocaine, both solids at room temperature, form a eutectic that's an oil with a 16°C melting point, used in
EMLA (Eutectic Mixture of Local Anesthetic) preparations.
Minerals may form eutectic mixtures in
igneous rocks, giving rise to characteristic
intergrowth textures such as that of
granophyre.
Some inks are eutectic mixtures, allowing
inkjet printers to operate at lower temperatures.
Other critical points
Eutectoid
When the solution above the transformation point is solid, rather than liquid, an analogous eutectoid transformation can occur. For instance, in the
iron-
carbon system, the
austenite phase can undergo a eutectoid transformation to produce
ferrite and
cementite (
iron carbide), often in
lamellar structures such as
pearlite and
bainite. This eutectoid point occurs at 727°C (1340.6 ºF) and about 0.83% carbon; alloys of nearly this composition are called
high-carbon steel, while those which have less carbon are termed
mild steel. The process analogous to glass formation in this system is the
martensitic transformation.
Peritectic
Peritectic transformations are also similar to eutectic reactions. Here, a liquid and solid phase of fixed proportions react at a fixed temperature to yield a single solid phase. Since the solid product forms at the interface between the two reactants, it can form a diffusion barrier and generally causes such reactions to proceed much more slowly than eutectic or eutectoid transformations. Because of this, when a peritectic composition solidifies it doesn't show the lamellar structure that you find with eutectic freezing.
Such a transformation exists in the
iron-
carbon system, as seen near the upper-left corner of the figure. It resembles an inverted eutectic, with the δ phase combining with the liquid to produce pure
austenite at 1495 °C and 0.17 mass percent carbon.
Further Information
Get more info on 'Eutectic Point'.
|
External Link Exchanges
Do you know how hard it is to get a link from a large encyclopaedia? Well we're different and will prove it. To get a link from us just add the following HTML to your site on a relevant page:
<a href="http://eutectic_point.totallyexplained.com">Eutectic point Totally Explained</a>
Then simply click through this link from your web page. Our crawlers will verify your link, extract the title of your web page and instantly add a link back to it. If you like you can remove the words Totally Explained and embed the link in article text.
As long as your link remains in place, we'll keep our link to you right here. Please play fair - our crawlers are watching. Your site must be closely related to this one's topic. Any kind of spamming, dubious practises or removing the link will result in your link from us being dropped and, potentially, your whole site being banned. |